摘要:
An object of the present invention is to provide a die-adhering adhesive film which can be laminated on a back of a wafer at a temperature lower than a softening temperature of a protecting tape for an ultra-thin wafer, or a dicing tape to be laminated, can reduce a thermal stress such as warpage of a wafer, can simplify a step of manufacturing a semiconductor device, and is excellent in heat resistance and humidity resistance reliance, an adhesive sheet in which the adhesive film and a dicing tape are laminated, as well as a semiconductor device.
摘要:
An object of the present invention is to provide a die-adhering adhesive film which can be laminated on a back of a wafer at a temperature lower than a softening temperature of a protecting tape for an ultra-thin wafer, or a dicing tape to be laminated, can reduce a thermal stress such as warpage of a wafer, can simplify a step of manufacturing a semiconductor device, and is excellent in heat resistance and humidity resistance reliance, an adhesive sheet in which the adhesive film and a dicing tape are laminated, as well as a semiconductor device.
摘要:
The method for producing a semiconductor chip with an adhesive film of the present invention comprises steps of preparing a laminate in which at least a divided semiconductor wafer comprising a plurality of semiconductor chips, obtained by forming a cut which separates the semiconductor wafer into a plurality of semiconductor chips on one side of the semiconductor wafer in a thickness less than that of the semiconductor wafer and by grinding the other side of the semiconductor wafer on which no cut is formed to reach the cut, an adhesive film for a semiconductor and a dicing tape are laminated, the adhesive film for a semiconductor having a thickness in the range of 1 to 15 μm and a tensile elongation at break of less than 5%, and the tensile elongation at break being less than 110% of the elongation at a maximum load; and dividing the adhesive film for a semiconductor by picking up the plurality of semiconductor chips in a laminating direction of the laminate, thereby preparing a semiconductor chip with an adhesive film.
摘要:
Disclosed is an adhesive composition which includes (a) an epoxy resin, (b) a curing agent and (c) a polymer compound incompatible with said epoxy resin, and further optionally includes (d) a filler and/or (e) a curing accelerator. Also disclosed are a process for producing an adhesive composition, including mixing (a) the epoxy resin and (b) the curing agent with (d) the filler, followed by mixing the resultant mixture with (c) the polymer compound incompatible with the epoxy resin; an adhesive film including the above-mentioned adhesive composition formed into a film; a substrate for mounting a semiconductor including a wiring board and the above-mentioned adhesive film disposed thereon on its side where chips are to be mounted; and a semiconductor device which includes the above-mentioned adhesive film or the substrate for mounting a semiconductor.
摘要:
A method for producing a semiconductor chip with an adhesive film, which includes: preparing a laminate in which a semiconductor wafer, an adhesive film and a dicing tape are laminated in that order, the adhesive film having a thickness in the range of 1 to 15 μm and a tensile elongation at break of less than 5%, and the tensile elongation at break being less than 110% of the elongation at a maximum load, and the semiconductor wafer having a section, for dividing the semiconductor wafer into a plurality of semiconductor chips, which is formed by irradiating with laser light; dividing the semiconductor wafer into a plurality of semiconductor chips without dividing the adhesive film, by expanding the dicing tape; and dividing the adhesive film by picking up the plurality of semiconductor chips.
摘要:
Disclosed is an adhesive composition which includes (a) an epoxy resin, (b) a curing agent and (c) a polymer compound incompatible with said epoxy resin, and further optionally includes (d) a filler and/or (e) a curing accelerator. Also disclosed are a process for producing an adhesive composition, including mixing (a) the epoxy resin and (b) the curing agent with (d) the filler, followed by mixing the resultant mixture with (c) the polymer compound incompatible with the epoxy resin; an adhesive film including the above-mentioned adhesive composition formed into a film; a substrate for mounting a semiconductor including a wiring board and the above-mentioned adhesive film disposed thereon on its side where chips are to be mounted; and a semiconductor device which includes the above-mentioned adhesive film or the substrate for mounting a semiconductor.
摘要:
There is an adhesive film for a semiconductor for use in a method for manufacturing a semiconductor chip. The method includes preparing a laminated body having a semiconductor wafer, an adhesive film for a semiconductor and dicing tape laminated in that order. The adhesive film for a semiconductor has a tensile breaking elongation of less than 5%, and the tensile breaking elongation is less than 110% of the elongation at maximum load. The semiconductor wafer is partitioned into multiple semiconductor chips and notches are formed from the semiconductor wafer side so that at least a portion of the adhesive film for a semiconductor remains uncut in its thickness direction. The method also includes stretching out the dicing tape in a direction so that the multiple semiconductor chips are separated apart, to separate the adhesive film for a semiconductor along the notches.
摘要:
There is provided a method for preparing dendrimer-modified magnetic fine particles wherein such particles can be made within a shorter time and more inexpensively than in the above-stated prior art processes and lot-to-lot variations in properties are lessened. The method for preparing dendrimer-fixed magnetic fine particles comprises the steps of providing magnetic particles having a functional group at a surface thereof, providing a dendrimer having a functional group at a base end portion thereof and synthesized to a desired generation and binding the functional group of the magnetic particles and the functional group of the dendrimer directly or indirectly through a crosslinking agent.
摘要:
The method for producing a semiconductor chip with an adhesive film of the present invention comprises steps of preparing a laminate in which at least a divided semiconductor wafer comprising a plurality of semiconductor chips, obtained by forming a cut which separates the semiconductor wafer into a plurality of semiconductor chips on one side of the semiconductor wafer in a thickness less than that of the semiconductor wafer and by grinding the other side of the semiconductor wafer on which no cut is formed to reach the cut, an adhesive film for a semiconductor and a dicing tape are laminated, the adhesive film for a semiconductor having a thickness in the range of 1 to 15 μm and a tensile elongation at break of less than 5%, and the tensile elongation at break being less than 110% of the elongation at a maximum load; and dividing the adhesive film for a semiconductor by picking up the plurality of semiconductor chips in a laminating direction of the laminate, thereby preparing a semiconductor chip with an adhesive film.
摘要:
The present invention provides a dicing/die bonding sheet which can be used as a dicing tape during dicing, enables ready separation of the semiconductor element and the adhesive layer from the pressure-sensitive adhesive layer during pickup, and in which the adhesive layer has satisfactory adhesiveness as a die bonding material. A dicing/die bonding sheet in which the pressure-sensitive adhesive layer comprises a compound (A), containing intramolecular, radiation curable carbon-carbon double bonds with an iodine value of 0.5 to 20, and at least one compound (B) selected from a group consisting of polyisocyanates, melamine-formaldehyde resins, and epoxy resins, and the adhesive layer comprises an epoxy resin (a), a phenolic resin (b) with a hydroxyl equivalent of at least 150 g/eq., an epoxy group-containing acrylic copolymer (c), comprising from 0.5 to 6% by weight of glycidyl acrylate or glycidyl methacrylate, and with a weight average molecular weight of at least 100,000, a filler (d), and a curing accelerator (e).