Abstract:
A method for producing a meta-aramid fiber paper-based material includes steps of: adding functional powders into a first poly(m-phenylene isophthalamide) solution, and obtaining a homogeneous mixed solution; through a dry spinning method, obtaining meta-aramid chopped fibers; through a second poly(m-phenylene isophthalamide) solution, obtaining meta-aramid fibrids; processing the fibrids with a multi-stage classification, selecting the fibrids having an appropriate mesh number and combining in proportion; mixing the chopped fibers and the fibrids, and relieving until uniform; forming a paper through an ultralow concentration inclined wire forming machine with an ultrasonic process and a wet-papermaking process; after squeezing and drying, obtaining a meta-aramid fiber base paper, and then processing with surface coating; and, after multi-stage calendering, rewinding and slitting, obtaining the high-performance meta-aramid fiber paper-based material. The paper-based material has a thickness of 1.5-30 mil, a high whiteness, a smooth and even surface, excellent characteristics, and a good performance stability.
Abstract:
Nonaqueous coating material compositions comprising at least one polyhydroxyl and (per)fluoroalkyl group-containing poly(meth)acrylate component (A), at least one polyisocyanate group-containing compounds (B), and one or more catalysts (D). Also provided are multistage coating methods using the coating material compositions, and also the use of the coating material compositions as a clearcoat material and for coating of wind energy systems or aircraft, or parts thereof, more particularly as an anti-icing coating.
Abstract:
The purpose of the present invention is to provide an additive for a solvent-based coating material which has high coating material product stability when added to a solvent-based coating material and whereby the resulting coating film has excellent abrasion resistance. Specifically, the present invention provides a silica composition containing silica coated with a cationic surfactant represented by a specific structure, and also provides a solvent-based coating material composition comprising the silica composition.
Abstract:
A solvent composition and method for making same is disclosed having a composition between 26 to 90 weight percent propionate, butyrate, or combination thereof and between 10 to 74 weight percent fluorinated solvent blend, wherein the fluorinated solvent blend includes t-DCE. A polymer solvent system is also disclosed incorporating the solvent composition and dissolved polymers, such as SEBS polymers. The solvent composition and polymer solvent system is minimally combustible or preferably nonflammable.
Abstract:
Hydroxypolyamides, hydroxypolyamide products, and post-hydroxypolyamides are disclosed as gel forming agents. Hydroxypolyamides and post-hydroxypolyamides are prepared from known methods. Hydroxypolyamide products are produced from a modified polymerization procedure which utilizes strong base for deprotonation of ammonium salts from the esterification of stoichiometrically equivalent polyacid:polyamine salts. The hydroxypolyamide products are capable of gel formation at lower concentrations than hydroxypolyamides and post-hydroxypolyamides from the known methods of preparation, and are therefore superior gel forming agents.
Abstract:
The mechanical properties of urea formaldehyde resins may be improved by incorporating therein polyvinyl alcohol. The polyvinyl alcohol may be incorporated during pre-mixing, mid mixing, and/or post mixing of the resin components. Resins prepared using polyvinyl alcohol are particularly desirable in articles requiring improved mechanical strength and water resistance, as compared to similar resins prepared without the polyvinyl alcohol such as shingles.
Abstract:
In an aspect, the present disclosure relates to a polyamide solution comprising an aromatic polyamide and a solvent, wherein a Young's modulus of at least one direction of a cast film produced by casting the polyamide solution on a glass plate is 3.0 GPa or more, and a tensile strength of the cast film is 100 MPa or more and 250 MPa or less. In another aspect, the present disclosure relates to a polyamide solution comprising an aromatic polyamide and a solvent, wherein a Young's modulus of at least one direction of a cast film produced by casting the polyamide solution on a glass plate is 3.0 GPa or more, and an aromatic polyamide of the polyamide solution has a constitutional unit represented by following general formulae (I) and (II).
Abstract:
A dispersion having from one to sixty percent by weight of total dispersion of a solids component dispersed in an organic continuous phase is useful as a coating for substrates. The solids component contains 40-95 weight-percent of a polyolefin containing only carbon and hydrogen and that has a number average molecular weight that is greater than 400 gram per mole, 5-40 weight-percent of an amine salt of a functionalized polyolefin; and 0-20 weight-percent of optional additives, wherein weight-percent is based on total weight of solids and wherein the dispersed particles have an average particle size of less than 35 micrometers and the organic phase is a dispersion support medium for the polyolefin and amine salt of a functionalized polyolefin.
Abstract:
Redispersible polymer powder compositions which include a polyglycol in admixture with a redispersible polymer powder (RDP), which powder includes a codried mixture of a carboxylated, water insoluble film-forming styrene butadiene polymer and a colloidal stabilizer, results in cement compositions having unexpectedly superior overall bonding strength and adhesion after water immersion. Use of the polyglycol provides good workability or ease of troweling during application. In addition, the RDP composition, which includes the RDP and the polyglycol, provides the cement-based composition with excellent abrasion resistance, surface appearance, and color. Also, the RDP composition provides for at least a 30% reduction, for example a 50% or more reduction in the amount of retarder or retardant employed in the dry mix formulation for cement compositions, such as self leveling flooring compounds or compositions, and cement-based tile adhesives.
Abstract:
A solvent composition and method for making same is disclosed having a composition between 26 to 90 weight percent propionate, butyrate, or combination thereof and between 10 to 74 weight percent fluorinated solvent blend, wherein the fluorinated solvent blend includes t-DCE. A polymer solvent system is also disclosed incorporating the solvent composition and dissolved polymers, such as SEBS polymers. The solvent composition and polymer solvent system is minimally combustible or preferably nonflammable.