摘要:
The present invention relates to a wear resistant iron-based powder, suitable for the production of pressed and sintered components, comprising 10-20% by weight of Cr, 0.5-5% by weight of Mo and 1-2% by weight of C. The powder is characterised in that it includes pre-alloyed water atomized iron-based powder particles and chromium carbide particles diffusion bonded onto said pre-alloyed powder particles. The invention also relates to a method of producing this powder.
摘要:
Disclosed herein are methods and processes for making FeRh/FePt nanostructures and the use of these FeRh—FePt nanostructures as a magnetic recording media.
摘要:
A method for producing a powder for a magnetic core, in which an alkoxide film formation step and a silicone resin film formation step are carried out to form an insulation film composed of an alkoxide film and a silicone resin film on the surface of a pure iron powder, wherein the alkoxide film formation step comprises immersing a pure iron powder in an alkoxide-containing solution which is prepared by mixing a Si alkoxide having at least one organic group having a polar group comprising at least one of N, P, S and O atoms and an Al alkoxide with a dehydrated organic solvent, and drying to remove the dehydrated organic solvent, thereby forming an alkoxide film comprising an Al—Si—O type composite oxide on the surface of the pure iron powder; and the silicone resin film formation step comprises immersing the pure iron powder having the alkoxide film formed thereon in a silicone resin-containing solution which is prepared by mixing a silicone resin with an organic solvent, and drying to remove the organic solvent, thereby forming a silicone resin film on the alkoxide film.
摘要:
Particles and manufacturing methods thereof are provided. The manufacturing method of the particle includes providing a precursor solution containing a precursor dissolved in a solution, and irradiating the precursor solution with a high energy and high flux radiation beam to convert the precursor to nano-particles. Particles with desired dispersion, shape, and size are manufactured without adding a stabilizer or surfactant to the precursor solution.
摘要:
A novel solution route has been developed that after heat-treatment to 500-600° C. under inert atmosphere, yields highly porous composites of nano-sized metal (Ni) particle inclusions in ceramics (Al2O3). Metal loadings could be made from 95% Ni. The metal inclusion sizes in the Ni—Al2O3 system with the 10 atom % Ni sample were 4-7 nm, while for the 75 atom % Ni sample they were 5-8 nm. It was shown that the 10 atom % Ni sample could be used as a catalyst for the conversion of CO2 and CH4 in the temperature range 550-700° C., while higher temperatures led to growth of the Ni particles and carbon poisoning over time. The solution routes could also be deposited as thin dense films containing
摘要:
Methods for discover of ceramic nanomaterial suitable for an application by preparing an array of first layer of electrodes and printing ceramic nanomaterial films on the electrodes. A second layer of electrodes is printed on the nanomaterial films of ceramics to form an electroded film array. The electroded film array is sintered. Properties of the sintered electroded film array are measured and one of the array elements with properties suited for the particular application is identified.
摘要:
A composite powder for a deposition of a composite coating comprises a nonmetallic component and a metallic component, the metallic component having an amorphous structure or a nanocrystalline structure. The metallic component may include an amorphous metallic alloy. The metallic alloy may include constituents having the amorphous structure. The metallic component may include a combination of the metallic alloy existing in the amorphous state and constituents of the amorphous metallic alloy in the amorphous state. The composite metal-ceramic powders are used for depositing composite coatings on a selected surface. Disclosed are several methods and systems for producing such composite powders. Disclosed are also several methods and systems for depositing composite coatings. Advantageously, the deposited coatings exhibit high corrosion resistance, high wear resistance, and excellent structural properties.
摘要:
A water-atomized iron-based powder is provided that is pre-alloyed with 0.75-1.1% by weight of Ni, 0.75-1.1% by weight of Mo and up to 0.45% by weight of Mn, and further including 0.5-3.0%, preferably 0.5-2.5% and most preferably 0.5-2.0% by weight of Cu, and inevitable impurities, the balance being Fe.
摘要:
An insulating magnetic metal particle includes a magnetic metal particle containing at least one metal selected from the group consisting of Co, Fe, and Ni and having a diameter of 5 to 500 nm, a first inorganic insulating layer made of an oxide that covers the surface of the magnetic metal particle, and a second inorganic insulating layer made of an oxide that produces a eutectic crystal by reacting together with the first inorganic insulating layer at the time of heating them, the second inorganic insulating layer being coated on the first inorganic insulating layer. A thickness ratio of the second inorganic insulating layer with respect to the first inorganic insulating layer is set so that the first inorganic insulating layer remains on the surface of the magnetic metal particle after producing the eutectic crystal.
摘要:
A core-shell structure with magnetic, thermal, and optical characteristics. The optical absorption band is tailorable by choice of the mixing ratio of the core/shell component to give the desired shell thickness. The core-shell structure is particularly suitable for biomedical applications such as MRI (magnetic resonance imaging) developer, specific tissue identification developer, and magnetic thermal therapy.