Abstract:
A coating composition for a lubricating coating film includes: (A) a phenolic resin (B) an epoxy resin having an epoxy equivalent weight of 600 to 4000; and (C) at least one type of solid lubricant. The epoxy equivalent weight is generally defined by the number average molecular weight per the number of epoxy groups in a single molecule. The coating composition has a weight ratio of component (A) to the total weight of component (A) and component (B) of at least 50 weight %. A lubricating coating film, formed from the coating composition, has a high level of flexibility on surfaces of various base materials.
Abstract:
A connecting element for a tubular component, the connecting element being overlaid with a coating including a principal layer constituted by a nickel-phosphorus alloy, a tubular component including one or more such connecting elements, and a method for producing such a connecting element.
Abstract:
In order to obtain a cold rolled steel sheet having excellent press formability, a cold rolled steel sheet has, on a surface thereof, an organic-inorganic composite film containing: an organic resin; and a crystalline layered material. The organic-inorganic composite film has an average film thickness of 0.10 to 2.0 μm and contains 0.5 part or more by weight of the crystalline layered material as a solid with respect to 100 parts by weight of a solid of the organic resin. The crystalline layered material preferably is, for example, a layered double hydroxide represented by [M2+1-xM3+x(OH)2][An−]x/n.zH2O, where: M2+ is one or more of Mg2+, Ca2+, Fe2+, Ni2+, and Zn2+; M3+ is one or more of Al3+, Fe3+, and Cr3+; and An− is one or more of OH−, CO32−, Cl−, and (SO4)2−.
Abstract:
A method and chemical composition and material structure for improving fretting wear in substrates, particularly carbon-carbon composite (CCC). The invention relates to trilayer coatings, comprising a base of hard ZrO2, a middle layer of Al2O3, and a top layer of lubricious ZnO. The coatings of the present invention exhibit conformality and pore-filling down to approximately 100 microns into a carbon-carbon composite to which they are applied. The methods for preparing the coatings include a chemical vapor infiltration route, such as an atomic layer deposition (ALD) process, to uniformly and conformally coat the porous and open structure of CCC with a solid lubricant trilayer of ZnO/Al2O3/ZrO2 that results in significant improvement (65%) in fretting wear.
Abstract translation:一种用于改善基材,特别是碳 - 碳复合材料(CCC)中的微动磨损的方法和化学组成和材料结构。 本发明涉及三层涂层,其包括硬的ZrO 2的基底,Al 2 O 3的中间层和光滑的ZnO的顶层。 本发明的涂层对于它们所应用的碳 - 碳复合材料显示出约100微米的共形和孔隙填充。 制备涂层的方法包括化学气相渗透途径,例如原子层沉积(ALD)工艺,以均匀和保形的方式用ZnO / Al 2 O 3 / ZrO 2的固体润滑剂三层膜覆盖CCC的多孔和开放结构,从而导致 轻微磨损显着改善(65%)。
Abstract:
A swash plate type compressor is arranged with a plurality of semispherical shoes and a disc shaped swash plate. A resin coating having a honeycomb structure is formed on a surface and a rear surface (sliding surface) of the swatch plate which slides with the shoe. An edge part (top end) of each of the multiple cylinder bodies which forms the resin coating layer are at the same plane and forms a sliding surface which slides with the shoe. In addition, an interior space of each cylinder body forms a storage part of a lubricant and a container part for foreign objects.The swash plate can be provided with excellent wear resistance, seizure resistance and lubrication retention.
Abstract:
A particulate composite lubricant for powder metallurgy comprises: first discrete particles comprising at least about 90 wt % of a fatty primary monoamide wax, being substantially free of fatty bisamide wax, and being at least partially coated with metal oxide nanoparticles and second metal-stearate free discrete particles comprising a fatty bisamide wax. A particulate composite lubricant for powder metallurgy can comprise: a Montan acid ester wax and at least one fatty amide wax comprising at least one of a fatty monoamide wax and a fatty bisamide wax.
Abstract:
The present invention provides a thermally conductive grease composition which scarcely increases in hardness during high-temperature heating and has a minimized reduction in growth, containing: (A) an organopolysiloxane including at least two alkenyl groups per molecule, the 25° C. kinetic viscosity being 5,000 to 100,000 mm2/s; (B) a hydrolysable methyl polysiloxane, trifunctional at one terminus, represented by general formula (1) (R1 is a C1-6 alkyl group, and a is an integer 5 to 100); (C) a thermally conductive filler having a thermal conductivity of 10 W/m·° C. or greater; (D) an organohydrogenpolysiloxane containing two to five hydrogen atoms directly bonded to a silicon atom (Si—H group) per molecule; (E) an adhesion promoter having a triazine ring and at least one alkenyl group per molecule; and (F) a catalyst selected from the group consisting of platinum and platinum compounds.
Abstract:
A cleaning blade lubricant including an acicular shape lubricant is provided. The cleaning blade lubricant is applied to a cleaning blade of an electrophotographic printing device for improving the cleaning performance of a cleaning blade of an electrophotographic printing device.
Abstract:
A swash plate type compressor is arranged with a plurality of semispherical shoes and a disc shaped swash plate. A resin coating having a honeycomb structure is formed on a surface and a rear surface (sliding surface) of the swatch plate which slides with the shoe. An edge part (top end) of each of the multiple cylinder bodies which forms the resin coating layer are at the same plane and forms a sliding surface which slides with the shoe. In addition, an interior space of each cylinder body forms a storage part of a lubricant and a container part for foreign objects.The swash plate can be provided with excellent wear resistance, seizure resistance and lubrication retention.
Abstract:
A sliding layer for a multi-layer bearing material that is free of lead. The sliding layer can include PTFE, sphalerite, and solid lubricants. The solid lubricants can include graphite and antimony oxide. In some embodiments, the sliding layer includes from 70 to 80 vol % PTFE, from 10-20 vol % sphalerite, and from 1 to 10 vol % solid lubricant (for example, graphite and antimony oxide).