LOAD BEARING SURFACE
    31.
    发明申请
    LOAD BEARING SURFACE 审中-公开
    负载轴承表面

    公开(公告)号:US20160214310A1

    公开(公告)日:2016-07-28

    申请号:US14881541

    申请日:2015-10-13

    Abstract: An elastomeric load hearing surface with different load support characteristics in different directions. In one embodiment, the surface includes an elastomeric membrane that is oriented in only a single direction, for example, by compression or stretching, In another embodiment, the surface includes mechanical structures, such as connectors and variations in thickness that vary the load support characteristics in different directions. In another embodiment, a surface is both oriented and includes mechanical structures.

    Abstract translation: 具有不同负载支持特性的弹性载荷听力表面。 在一个实施例中,表面包括仅在单个方向上定向的弹性体膜,例如通过压缩或拉伸。在另一个实施例中,表面包括机械结构,例如连接器和厚度变化,其改变负载支撑特性 在不同的方向 在另一个实施例中,表面被定向并且包括机械结构。

    POLYAMIDE FILMS AND PROCESS FOR PREPARATION
    32.
    发明申请
    POLYAMIDE FILMS AND PROCESS FOR PREPARATION 有权
    聚酰胺薄膜和制备方法

    公开(公告)号:US20160183368A1

    公开(公告)日:2016-06-23

    申请号:US14910093

    申请日:2014-07-09

    Abstract: The invention relates to a stretched polymer film made of a polyamide composition comprising a semi-crystalline semi-aromatic polyamide (PPA), wherein the PPA consists of repeat units derived from aromatic dicarboxylic acid comprising at least 80 mole % of terephthalic acid, relative to the total amount of aromatic dicarboxylic acid; and diamine comprising at least 5 mole % 1,4-butanediamine and at least 5 mole % 1,6-hexanediamine, relative to the total amount of diamine, the combined amount of 1,4-butanediamine and 1,6-hexanediamine being at least 60 mole % relative to the total amount of diamine; and 0-2 mole % of other monomeric units, relative to the total amount of aromatic dicarboxylic acid, diamine and other monomeric units. The invention further relates to a process for preparing the polyamide film by melt extrusion and stretching of the film.

    Abstract translation: 本发明涉及由包含半结晶半芳族聚酰胺(PPA)的聚酰胺组合物制成的拉伸聚合物膜,其中PPA由衍生自包含至少80摩尔%对苯二甲酸的芳族二羧酸的重复单元组成,相对于 芳族二羧酸的总量; 和相对于二胺的总量,包含至少5摩尔%1,4-丁二胺和至少5摩尔%1,6-己二胺的二胺,1,4-丁二胺和1,6-己二胺的合并量为 相对于二胺的总量为至少60摩尔% 和0-2摩尔%的其它单体单元,相对于芳族二羧酸,二胺和其它单体单元的总量。 本发明还涉及一种通过熔融挤出和拉伸薄膜来制备聚酰胺薄膜的方法。

    Biaxially oriented polyethylene terephthalate film and method for producing same
    35.
    发明授权
    Biaxially oriented polyethylene terephthalate film and method for producing same 有权
    双轴取向聚对苯二甲酸乙二醇酯薄膜及其制造方法

    公开(公告)号:US09212268B2

    公开(公告)日:2015-12-15

    申请号:US14396295

    申请日:2013-07-19

    Abstract: This film provides a polyethylene terephthalate film whereby dimensional variation in various steps can be reduced, particularly when the film is used as a substrate film for a flexible device, and that is suitable as a substrate film having minimal curl and excellent appropriateness for processing. This biaxially oriented polyethylene terephthalate film has a degree of crystallinity (Xc) of 0.35 to 0.50, the intrinsic viscosity (IV) of the resin constituting the film is 0.66-1.0 dl/g, the coefficient of thermal expansion at a temperature of 50-170° C. in each of the machine direction and transverse direction of the film is 0.29 ppm/° C., and the degree of thermal shrinkage at 180° C. in each of the machine direction and transverse direction of the film is 0.5%-1.0%.

    Abstract translation: 该薄膜提供聚对苯二甲酸乙二醇酯薄膜,从而可以降低各步骤的尺寸变化,特别是当该薄膜用作柔性装置的基材薄膜时,适合作为具有最小卷曲和优异的加工适当性的基材薄膜。 该双轴取向聚对苯二甲酸乙二醇酯膜的结晶度(Xc)为0.35〜0.50,构成膜的树脂的特性粘度(IV)为0.66〜1.0dl / g,温度为50〜 膜的纵向和横向各自为170℃,为0.29ppm /℃,膜的纵向和横向各自的180℃下的热收缩率为0.5% -1.0%。

    METHOD OF PREPARING RETARDATION FILM, POLARIZING PLATE, AND LIQUID CRYSTAL DISPLAY
    38.
    发明申请
    METHOD OF PREPARING RETARDATION FILM, POLARIZING PLATE, AND LIQUID CRYSTAL DISPLAY 审中-公开
    制备薄膜,极化板和液晶显示的方法

    公开(公告)号:US20150114257A1

    公开(公告)日:2015-04-30

    申请号:US14398311

    申请日:2013-04-26

    Inventor: Takahiro Takagi

    Abstract: A method of preparing a retardation film includes cellulose acetate having an average degree of acetylation of 2.0 to 2.5 and having a moisture content of 1.0 mass % or less, where the retardation film includes a compound having a Van der Waals volume of 450 to 1000 Å3. The retardation film is prepared by a dope preparing step of dissolving cellulose acetate having an average degree of acetylation within the range of 2.0 to 2.5 to prepare a dope; a film product forming step of casting the dope onto a metal belt to form a film product; a film product peeling step of peeling off the film product from the metal belt; a drawing step of drawing the peeled film product; and a drying step at a drying temperature of 140° C. or more.

    Abstract translation: 制备延迟膜的方法包括平均乙酰化度为2.0〜2.5,水分含量为1.0质量%以下的乙酸纤维素,其中相位差膜包括范德华体积为450〜1000的化合物 。 相位差膜是通过将平均乙酰化度的乙酸纤维素溶解在2.0〜2.5的范围内的涂料制备工序来制备的。 将所述涂料浇铸到金属带上以形成膜产品的膜产品形成步骤; 从金属带剥离薄膜产品的薄膜产品剥离步骤; 拉伸剥离的薄膜制品的拉伸步骤; 干燥温度为140℃以上的干燥工序。

    Method For Producing Air-Permeable Composite Sheet
    40.
    发明申请
    Method For Producing Air-Permeable Composite Sheet 审中-公开
    生产透气复合片材的方法

    公开(公告)号:US20150040764A1

    公开(公告)日:2015-02-12

    申请号:US14523995

    申请日:2014-10-27

    Inventor: Hiroshi Manabe

    Abstract: It is an objective of the present invention to provide a method for producing an air-permeable composite sheet which has excellent mechanical strength and compression resistance as well as PTFE's innate property such as air-permeability, water repellency, heat resistance and chemical resistance; and a filter and a fabrics material containing the air-permeable composite sheet produced by the method as a constituent material. The method for producing an air-permeable composite sheet according to the present invention is characterized in comprising steps of filling pores of a porous PTFE sheet with a hardenable material solution; hardening or semi-hardening the porous PTFE sheet filled with the hardenable material solution; and expanding the hardened or semi-hardened porous PTFE sheet.

    Abstract translation: 本发明的目的是提供一种机械强度和抗压缩性优异的透气性复合片材的制造方法以及透气性,防水性,耐热性和耐化学性等PTFE的先天性质。 以及包含通过该方法制造的透气性复合片材的过滤器和织物材料作为构成材料。 根据本发明的透气性复合片的制造方法的特征在于,包括用可硬化材料溶液填充多孔PTFE片的孔的步骤; 硬化或半硬化填充有可硬化材料溶液的PTFE多孔板; 并膨胀硬化或半硬化的多孔PTFE片材。