Abstract:
The present invention relates to a permanently attached UHF band RFID tire tag and a manufacturing method thereof, and more specifically, the present invention relates to a permanently attached UHF band RFID tire tag and a manufacturing method thereof, which is attached to a tire surface during the manufacturing process of a tire in a high-temperature and high-pressure environment, enabling the management of tire manufacturing history from the beginning of the production to product shipment, and thereafter, the durability is maintained even in the flexing motion of a tire that occurs while the tire is installed and operated in a vehicle such that chip damage of a tag and tag detachment from the tire do not occur, and therefore, it enables RFID communication to be performed without obstacles until the end of a tire life.
Abstract:
A colored adhesive tape (1), in particular a yellow, orange-colored, or black adhesive tape (1), preferably a cable wrapping tape, with a temperature class of at least T3 (LV 312), including a textile substrate with a polymer plastic substrate (4, 4a, 4b), on which an adhesive material (5, 5a, 5b) is applied. In order to improve the temperature stability of the tape, while maintaining advantageous properties, the color of at least a part of the substrate (4, 4a, 4b) is formed by the inherent color of the polymer plastic material. The tape is preferably substrate formed of a polymer plastic materials which are aromatic, nitrogen-containing polymers from the group of polyoxadiazoles (POD), polybenzobisoxazoles (PBO) or polybenzimidazoles (PBI) (4, 4a, 4b). The adhesive tape (1) may be used as a cable harness (3).
Abstract:
Provided are methods of forming thermally conductive flexible bonds for use in electronic boards of unmanned spacecrafts and other types of aircraft. Also provided are methods of preparing adhesive materials to form these bonds including methods of preparing treated filler particles. In some aspects, an adhesive material includes filler particles having organofunctional groups, such as boron nitride particles treated in silane. These particles may be combined with a urethane modified epoxy to form the adhesive material. The weight ratio of the particles in the adhesive material may be about 40-60%. The adhesive material may be thermally cured using a temperature of less than 110° C. to prevent damage to bonded electronic components. The cured adhesive may have a thermal conductivity of at least about 2 W/m K measured in vacuum and may have a glass transition temperature if less than −40° C.
Abstract:
A novel silicone-acrylic copolymer which comprises a covalently bonded silicone polymer with an acrylic polymer through the —Si—O—Si— linkage is described. The silicone-acrylic copolymer is a reaction product of (a) a silicone polymer, (bi) a mixture of acrylic monomers wherein at least one acrylic monomer comprises a silane (meth)acrylic monomer and/or a siloxane (meth)acrylic macromer with a radical initiator to form an acrylic prepolymer or (bii) an acrylic polymer which comprises a silane or a siloxane functional group; and (c) a scrambling catalyst, wherein the ratio of the silicone polymer (a) and the mixture of acrylic monomers (bi) or polymer (bii) is from 50:1 to 1:50. The silicone-acrylic copolymer is useful as an adhesive, sealant, coating, and the like.
Abstract:
Embodiments of the invention provide a robust bonding material suitable for joining semiconductor processing chamber components. Other embodiments provide semiconductor processing chamber components joined using an adhesive material with desired characteristics. In one embodiment, an adhesive material suitable for joining semiconductor chamber components includes an adhesive material having a Young's-modulus lower than 300 psi. In another embodiment, a semiconductor chamber component includes a first surface disposed adjacent a second surface, and an adhesive material coupling the first and second surfaces, wherein the adhesive material has a Young's modulus lower than 300 psi.
Abstract:
The invention relates to a crosslinkable one-component laminating adhesive containing 25 to 80 wt. % of polyester prepolymers, polyether prepolymers and/or polyurethane prepolymers, which have at least two cross-linkable alkoxysilane groups and have a molecular weight of 2000 to 30,000 g/mol, 75 to 19 wt. % of organic solvent having a boiling point up to 130° C., 1 to 20 wt. % of polymers which contain anhydride groups, and 0 to 15 wt. % of additives, wherein the viscosity of the adhesive is between 50 and 20,000 mPas (according to DIN ISO 2555), measured at 15 to 45° C.
Abstract translation:本发明涉及一种含有25〜80wt。 具有至少两个可交联烷氧基硅烷基并且分子量为2000至30,000g / mol,75至19wt。%的聚酯预聚物,聚醚预聚物和/或聚氨酯预聚物的百分比。 %的沸点高达130℃的有机溶剂,1〜20重量% 含有酸酐基团的聚合物的%,和0至15wt。 %的添加剂,其中在15至45℃下测量粘合剂的粘度为50至20,000mPas(根据DIN ISO 2555)。
Abstract:
The present invention relates to an adhesive film and to a touch panel. According to the present invention, even when the adhesive film is applied to a touch panel, for example, a capacitive touch panel, and directly attached to a conductive layer, the adhesive film effectively prevents the resistance of the conductive layer from being raised and exhibits good heat resistance. In addition, according to the present invention, an adhesive film having superior durability, optical characteristics, cuttability, workability, wettability and resistance to warping is provided.
Abstract:
An adhesive based on casein, water-soluble extenders, natural or synthetic resin acids, resin alcohols or resin esters, and an alcohol is provided. The adhesive has specific amounts of these ingredients which leads to a viscosity of the adhesive which is temperature dependent to a surprisingly large extent. The adhesive is particularly useful in the labelling of bottles wherein the surface of the bottles is wet and cold.
Abstract:
The invention relates to a crosslinkable one-component laminating adhesive containing 25 to 80 wt. % of polyester prepolymers, polyether prepolymers and/or polyurethane prepolymers, which have at least two cross-linkable alkoxysilane groups and have a molecular weight of 2000 to 30,000 g/mol, 75 to 19 wt. % of organic solvent having a boiling point up to 130° C., 1 to 20 wt. % of polymers which contain anhydride groups, and 0 to 15 wt. % of additives, wherein the viscosity of the adhesive is between 50 and 20,000 mPas (according to DIN ISO 2555), measured at 15 to 45° C.
Abstract:
A transparent adhesive sheet for optics, which is capable of satisfying both adhesion and rework property, in view of the above problems of prior art. A production method of a silicone-based transparent adhesive sheet for optics for assembling the optical components, includes a step of forming a surface activation treated surface, in which peel strength after laminating onto an adherend increases with time, as compared with peel strength before lamination. The surface activation treatment is performed by using UV-ray irradiation on at least a part or the entire surface of an adhesive face contacting with the adherend of said transparent adhesive sheet for optics.