Methods for stud bump formation and apparatus for performing the same
    3.
    发明授权
    Methods for stud bump formation and apparatus for performing the same 有权
    螺栓凸块形成方法及其执行方法

    公开(公告)号:US08540136B1

    公开(公告)日:2013-09-24

    申请号:US13605403

    申请日:2012-09-06

    IPC分类号: B23K31/02 B23K37/00

    摘要: Methods for forming stud bumps and apparatuses for forming stud bumps are disclosed. According to an embodiment, a method includes clamping a wire with a clamp. The clamp includes at least two opposing plates, and at least one of the opposing plates includes a protruding feature that intersects the wire when the wire is clamped forming a first notch in the wire. The method further includes bonding the wire to a bonding surface, releasing the wire from the clamp, passing the wire a notch pitch distance through the clamp, clamping the wire with the clamp forming a second notch in the wire, and breaking the wire leaving a bonded portion of the wire on the bonding surface. The second notch is the notch pitch distance from the first notch along the wire.

    摘要翻译: 公开了用于形成柱形凸块的方法和用于形成凸块凸块的装置。 根据实施例,一种方法包括用夹具夹紧线。 所述夹具包括至少两个相对的板,并且当所述线被夹紧形成所述线中的第一凹口时,所述相对板中的至少一个包括与所述线相交的突出特征。 该方法还包括将线接合到接合表面,将线从夹具中释放出来,使线穿过钳口的间距距离通过夹具夹紧线,夹具在线中形成第二凹口,并将线断开, 接合表面上的导线的接合部分。 第二个凹口是距离第一个凹口沿导线的切口间距距离。